Keywords: nanoindentation

Microstructure and Pile-up effect on Nanoindentation measurements of FCC and BCC Metals

Srivastava A.K., Mirshams R.A., University of North Texas, US
A study of effects of crystal orientation and pile-up on mechanical properties of Fe, Ni and Cu is made.

Comparison between Nanoindentation and Scratch Test Hardness (Scratch Hardness) Values of Copper Thin Films on Oxidised Silicon Substrates

Chowdhury S., Beegan D., Laugier M.T., University of Alabama at Birmingham, US
We have measured hardness i.e. scratch hardness from the scratch tester usually used for investigating adhesion in thin films and compare this with hardness measured by the nanoindentation technique on copper thin films. We defined [...]

Microfabrication and Mechanical Characterization of Suspended Carbon Microstructures

Malladi K., Wang C., Madou M.J., Xue W., Cui T., University of California Irvine, US
The idea of suspended carbon micro/nanostructures has been researched by a few research groups ], however, controlled fabrication of suspended carbon micro/nano structures in desired positions and with the desired shape and dimension is still [...]

Multi-scale Discrete Dislocation Plasticity Analysis: Application to Nano-indentation

Khan S.M.A., Levine L.E., National Institute of Standards and Technology, US
With the growing utilization of nano-scale components in various technologies like MEMS, NEMS, thin films, medical diagnostics etc, nano-indentation testing is finding new expanding applications towards quantitative determination of mechanical properties at the nano-scale. In [...]

Reliability of Atomistic-Continuum Modeling Simulations for Problems in Molecular Statics

Prudhomme S., Bauman JP., Oden J.T., The University of Texas at Austin, US
Multi-scale computational modeling aims at developing systematic techniques for bridging scales between atomistic models and continuum models in order to increase the speed of dynamical calculations. Continuum level models can simulate large volumes of material, [...]

Nanomechanical Properties of Silica Coated Multiwall Carbon Nanotubes – Poly(methyl methacrylate) Composites

Olek M., Kempa K., Jurga S., Giersig M., Caesar - Research Center, DE
Nanomechanical properties of polymer composites, reinforced with silica coated multiwall carbon nanotubes (MWNT), have been studied using the nanoindentation technique. The nanohardness and the Young’s modulus have been found to increase strongly with the increasing [...]

Elasto-plastic Properties of Electroplated and Polycrystalline Nickel using Numerical Modelling of the Nanoindentation Test Coupled with an Inverse Method

Qasmi M., Delobelle P., Richard F., Université de Franche-Comté, FR
The aim of this paper is a wide investigation of the nano scale of the elastoplastic properties of electroplated Nickel, which is extensively used in the LIGA techniques and polycrystalline hardened and annealed Nickel with [...]

Orientation E®ects of Elastic-Plastic Deformation at Surfaces: Nanoindentation of Nickel Single Crystals

Kum O., Clemson University, US
Orientation effects in nanomechanical properties at the surfaces with molecular dyanmics were observed as a function of indenter size and indenter speed in three crystal orientations: 100, 110, and 111. The force vs displacement curves [...]

Theoretical Strength and Onset of Yielding in Nanoindentation

Sob M., Friák M., Vitek V., Academy of Sciences of the Czech Republic, CZ
Quantum-mechanical (ab initio) approach for determining theoretical (ideal) tensile and shear strength in metals and intermetallics is briefly outlined and as an example, tensile test for defect-free MoSi2 is simulated. Theoretical values of tensile and [...]

Posts pagination

« 1 2

About TechConnect Briefs

TechConnect Briefs is an open access journal featuring over 10,000 applications-focused research papers, published by TechConnect and aligned with over 20 years of discovery from the annual Nanotech and the TechConnect World Innovation Conferences.

Full Text Search

TechConnect World

June 17-19, 2024 • Washington, DC

TechConnect Online Community

» Free subscription!

Topics

3D Printing Advanced Manufacturing Advanced Materials for Engineering Applications AI Innovations Biofuels & Bioproducts Biomaterials Cancer Nanotechnology Carbon Capture & Utilization Carbon Nano Structures & Devices Catalysis Chemical, Physical & Bio-Sensors Coatings, Surfaces & Membranes Compact Modeling Composite Materials Diagnostics & Bioimaging Energy Storage Environmental Health & Safety of Nanomaterials Fuel cells & Hydrogen Graphene & 2D-Materials Informatics, Modeling & Simulation Inkjet Design, Materials & Fabrication Materials Characterization & Imaging Materials for Drug & Gene Delivery Materials for Oil & Gas Materials for Sustainable Building MEMS & NEMS Devices, Modeling & Applications Micro & Bio Fluidics, Lab-on-Chip Modeling & Simulation of Microsystems Nano & Microfibrillated Cellulose Nanoelectronics Nanoparticle Synthesis & Applications Personal & Home Care, Food & Agriculture Photonic Materials & Devices Printed & Flexible Electronics Sensors - Chemical, Physical & Bio Solar Technologies Sustainable Materials Water Technologies WCM - Compact Modeling
MENU
  • Sitemap
  • Contact
  • Sitemap
  • Contact

Copyright © TechConnect a Division of ATI | All rights reserved.