Epoxy/Silica Nanocomposite: Effect of Silica Nanoparticles, Thermal Stability, and Modeling of the Curing Kinetics

Rahim Vaseghi M., Arabli V., Aghili A., Islamic Azad University, IR
A nanocomposite was synthesized using silica nanoparticles (SN) and Epoxy Vinyl Ester Resin (VE671). Nanoparticles were dispersed in the mixture by ultrasonic equipment to prevent the agglomeration. Transmission electron microscopy (TEM) was used to investigate [...]

Generation of Transportation Fuel from Solid Municipal Waste Plastics

Sarker M., Natural State Research, Inc., US
Transportation fuels derived from imported fossil fuels are subjected to the price fluctuations of the global marketplace, and constitute a major expense in the operation of a vehicle. Emissions from the evaporation and combustion of [...]

Generation of Transportation Fuel from Solid Municipal Waste Plastics

Sarker M., Natural State Research, Inc., US
Transportation fuels derived from imported fossil fuels are subjected to the price fluctuations of the global marketplace, and constitute a major expense in the operation of a vehicle. Emissions from the evaporation and combustion of [...]

About TechConnect Briefs

TechConnect Briefs is an open access journal featuring over 10,000 applications-focused research papers, published by TechConnect and aligned with over 20 years of discovery from the annual Nanotech and the TechConnect World Innovation Conferences.

Full Text Search

TechConnect World

June 17-19, 2024 • Washington, DC

TechConnect Online Community

» Free subscription!

Topics

3D Printing Advanced Manufacturing Advanced Materials for Engineering Applications AI Innovations Biofuels & Bioproducts Biomaterials Cancer Nanotechnology Carbon Capture & Utilization Carbon Nano Structures & Devices Catalysis Chemical, Physical & Bio-Sensors Coatings, Surfaces & Membranes Compact Modeling Composite Materials Diagnostics & Bioimaging Energy Storage Environmental Health & Safety of Nanomaterials Fuel cells & Hydrogen Graphene & 2D-Materials Informatics, Modeling & Simulation Inkjet Design, Materials & Fabrication Materials Characterization & Imaging Materials for Drug & Gene Delivery Materials for Oil & Gas Materials for Sustainable Building MEMS & NEMS Devices, Modeling & Applications Micro & Bio Fluidics, Lab-on-Chip Modeling & Simulation of Microsystems Nano & Microfibrillated Cellulose Nanoelectronics Nanoparticle Synthesis & Applications Personal & Home Care, Food & Agriculture Photonic Materials & Devices Printed & Flexible Electronics Sensors - Chemical, Physical & Bio Solar Technologies Sustainable Materials Water Technologies WCM - Compact Modeling
  • Sitemap
  • Contact

Copyright © TechConnect a Division of ATI | All rights reserved.