Fabrication chitosan nano fibers membrane via electrospinning
Chitosan nanofibers were prepared via electrospinning by varying solution concentration (1, 2, 4 and 6wt %), applied voltage (14, 18 and 22 kV), distance between needle and collector (100 mm and 140 mm), needle diameter [...]